how to make rubber pad

1. cleaning printing head mould, then putting it on balanceable
2. dipping into silastic and silicon oil proportionally

3. stiring, making it well-distribut
4. adding hardener proportionally

5. stiring fully again, then lasting 5 minutes to remove bubbles
6. putting the stired liquid into printing head mould slowing, in order to avoid bubbles, when putting you should be slow

7. after pouring all the liquid, covering wood, Generally 3-4 hours later, it will be demould.
8. finishing, taking out the printing he